Description
Differential Scanning Calorimeters (DSC) measures temperatures and heat flows associated with thermal transitions in a material. Properties that can be investigated include, glass transitions, “cold†crystallization, phase changes, melting, crystallization, product stability, cure / cure kinetics, and oxidative stability.Features
- Temperature range, -90 to 400°C, with precision of 0.05°C
- Sensitivity of 0.2 µW with 50 position autosampler
- Ideal for Tg, Tm, and Cp measurements